Is cooling rate important for sub-critical anneal?

A board dedicated to advanced metallurgical bladesmithing methods.

Is cooling rate important for sub-critical anneal?

Postby Alexander B » Wed Jan 10, 2018 12:11 am

With most of my knives, I include a quench as part of my last grain-refining thermal cycle, followed by a 2-hour sub-critical anneal at 1200 F. After the 2-hour soak, should I remove the blades and allow to air cool, or turn of the kiln and leave the blades inside? Or does it not matter?

Apologies if this has been answered in other posts!
Alexander B
Regular
 
Posts: 57
Joined: Sat Sep 20, 2014 2:39 pm

Re: Is cooling rate important for sub-critical anneal?

Postby Kevin R. Cashen » Wed Jan 10, 2018 11:28 am

I am pretty sure that two hours is enough for equilibrium to be reached, cooling rate should be irrelevant.
Everybody has the privilege of settling on their own level of ignorance. Nobody has the right to impose it on others.
User avatar
Kevin R. Cashen
Professional Bladesmith
 
Posts: 956
Joined: Thu Aug 06, 2009 11:36 pm
Location: Hubbardston, MI

Re: Is cooling rate important for sub-critical anneal?

Postby Robert C » Tue Feb 13, 2018 1:09 am

That should do it !
Robert C
Resident Metallurgist
 
Posts: 607
Joined: Wed Oct 07, 2009 6:51 pm